Lahane
Mechanical
- Jul 23, 2010
- 27
I have a qualified SS PQR as follows with impact test
Material: SA 312 TP 316L to SA 312 TP 316L(P8G1 TO P8G1)
Process: GTAW with ARGON gas purging
Consumable:ER 316L Filler wire
position : 6G
Thickness: 8.2 mm
By using above PQR, I have developed new WPS with impact test to weld 12.7 mm thick A 312 TP 321 pipe to A182 F 321 flange by using ER347 filler wire.
The WPS was submitted to customer & it was got rejected.Can any body highlight what could be the cause of rejection???
Material: SA 312 TP 316L to SA 312 TP 316L(P8G1 TO P8G1)
Process: GTAW with ARGON gas purging
Consumable:ER 316L Filler wire
position : 6G
Thickness: 8.2 mm
By using above PQR, I have developed new WPS with impact test to weld 12.7 mm thick A 312 TP 321 pipe to A182 F 321 flange by using ER347 filler wire.
The WPS was submitted to customer & it was got rejected.Can any body highlight what could be the cause of rejection???