SS 347 consumables are used to weld the ss 321 parts. What is the reason that generally ss 321 consumables are not used/made for welding of SS 321 parts?

 
Replies continue below

Recommended for you

Loss of Ti through the arc. 321 can be used in GTAW process.
 