OSUCivlEng

Civil/Environmental
Jan 12, 2009
275
I recently designed a new steel bridge on a 45 degree skew with staggered cross frames. I received a comment from the DOT reviewer that this increases the possibility of fatigue cracks. I was puzzled by this comment, as everything I have read says that staggered cross frames reduces cross frame forces. If you reduce the connection force shouldn't the magnitude of the stress go down? I do understand that it increases the lateral bending in the flanges.

 
Replies continue below

Recommended for you

Thanks. I'm well aware of that document. Apparently they have had several plate girders with staggered cross frames develop some pretty large cracks. After seeing the evidence I am not really convinced it's the staggered bracing. They may be open to adding an additional stiffener on the opposite side of the web at cross frame connection locations.
 
An additional stiffener was my thought also. Question: Are the cross frame connection plates welded to the tension flange or do you provide a tab plate?
 
Yes they are welded to the tension flange. I have seen details for a tab plate, but I'm not aware of them ever being used in this state.
 
Tab plates & bolting the stiffener to the tension flange with angles is common in the northeast.
 
Does the DOT have a preferred detail or preferred crossframe layout?
 