Is it permissible to use F563C, F593D, F593G, and F593H bolts in a Div.1 PV?
Thanks!
 
Replies continue below

Recommended for you

I use the following stainless hardware when designing in accordance with ASME Section VIII, Div.1:

304 SS bolting = SA-193-B8

316 SS bolting = SA-193-B8M

I have never used any of the designations you have listed for pressure vessel design.
 