Can anyone advise as to what the minimum Yield is for stainlees steel 316L?

Many Thanks,

Dave.
 
Replies continue below

Recommended for you

Refer Metals Handbook or do a Google search.

_____________________________________
"It's better to die standing than live your whole life on the knees" by Peter Mayle in his book A Good Year
 
Thanks Armunmrao, i already googled and i got 170Mpa. However being a novice i wasn't confident it was the right answer.

TVP - thanks for the PDF, very useful..
 
In ASTM specs it is listed as 25ksi (170MPa) with a UTS or 70ksi (485MPa)

= = = = = = = = = = = = = = = = = = = =