I have an analysis of the following metal whose source I am trying to identify
17.3 Cr
1.5 Mn
0.47 Ni
0.43 Si
0.11 Al ? (is this real or contamination)
0.0 Mo
it doesnt quite fit with any of the grades that I can check against.
Also is there a single listing of all AISI grade chemical compositions
thanks
Kevin