Dear guys. Is it possible to have an stainless steel (austenitic) with a carbon percentage of 0.20%? I have never seen such high content since I remember that less than 0,10% carbon content is normal.
 
Replies continue below

Recommended for you

I don't know of any H grade 300 alloys that are over 0.10% C.
There are higher C cast grades for high temp service.
All of the H- grades are 0.20% and higher.
Remember that C is an austenite stabilizer.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
Most of the cast grades of heat resistant alloys have carbon above 0.20 ( ASTM A 297).

 