dhdz187
Mechanical
- Apr 12, 2010
- 7
We are serving an aluminum parts for our customer, it is a part that used in hard disk industry. the material is AL6061-T6 and beadblast is required at customer side after all machining process finished. We only do machining process,and beadblast is done by customer.
The problem now is that some stains was found on the surface of the part after beadblast and drying process. Below is the photo:
Stains was found on the surface near the blind holes (8-32 UNC threaded hole).
It must be strongly emphasized that stains only be found after beadblast and drying process. It looks nice before these process.
Here is something to share, it is what we are doing now :
Only water-soluble cutting fluid is allowed during machining process and ultrasonic cleaning was followed before shipment to customer, we even check all blind holes with a cotton swab.
We are making efforts to improve our cleaning process continuously, but problem still can't be solved.
What 's the probable root cause?
Ultrasound frequencies? Ultrasonic cleaning temperature? or cleaning solvent is not suitable? or other cause?
Any comment will be appreciated.
The problem now is that some stains was found on the surface of the part after beadblast and drying process. Below is the photo:
Stains was found on the surface near the blind holes (8-32 UNC threaded hole).
It must be strongly emphasized that stains only be found after beadblast and drying process. It looks nice before these process.
Here is something to share, it is what we are doing now :
Only water-soluble cutting fluid is allowed during machining process and ultrasonic cleaning was followed before shipment to customer, we even check all blind holes with a cotton swab.
We are making efforts to improve our cleaning process continuously, but problem still can't be solved.
What 's the probable root cause?
Ultrasound frequencies? Ultrasonic cleaning temperature? or cleaning solvent is not suitable? or other cause?
Any comment will be appreciated.