brixtontech
Mechanical
- Apr 14, 2009
- 1
I need to stamp parts from annealed C-110 copper strip that is 0.005" thick and hot tin-dipped to 0.0005" thick both sides. The part dimensions are roughly 0.5" x 3.5", and the production volume is around 20 million pieces. Because of down-stream processing of the part I would strongly prefer to stamp the strip without any lubricant. Does anyone have any experience dry stamping this material - or any suggestions on die materials to reduce tooling wear?