Dear,
We have encountered a problem with an impeller in an vessel.
What is the standard blade thickness of a pitched blade impeller?
Impeller: pitched blade 45deg, 6-blades
Impeller diameter: 600 mm
Vessel diam: 1800 mm
Power input: 17 kW
Max. Vol. 4.7 m3
Speed = 265 rpm max
We have 6 mm, but blades simply sheared off (so might be not sufficient strength)
There was no abnormal unblance/wobbling of the shaft.
MoC: 316L
Shaft length: 2500 mm, Shaft thickness: 110 mm
We don’t understand why blades sheared off. First idea is blade thickness to small.
Kind regards,
John
We have encountered a problem with an impeller in an vessel.
What is the standard blade thickness of a pitched blade impeller?
Impeller: pitched blade 45deg, 6-blades
Impeller diameter: 600 mm
Vessel diam: 1800 mm
Power input: 17 kW
Max. Vol. 4.7 m3
Speed = 265 rpm max
We have 6 mm, but blades simply sheared off (so might be not sufficient strength)
There was no abnormal unblance/wobbling of the shaft.
MoC: 316L
Shaft length: 2500 mm, Shaft thickness: 110 mm
We don’t understand why blades sheared off. First idea is blade thickness to small.
Kind regards,
John