If I were to design a steel joist. And by this I mean structurally design the joist, not lay them out for a building, but actually designing the top chord, web and bottom chord. What would be the code checks to follow from the AISC code book?
For a K series joist I want to use the following:
Top Chord: Double Angles (Equal lengths)36 Ksi
Web: Single Angle (Uncrimped-First analysis, Crimped-Second Analysis)36 Ksi
Bottom Chord: Double Angles (Equal lengths) 36 KSI
Rods at each ends from bottom chord to top chord.
The Vulcraft Manual states the bottom chord to be checked in axial tension only, web in compression, and top chord in axial compression ONLY if panels are less than 24" apart.
I've used Chapters D,E,and F.
D2
E3 & E4
F9
When I asked my boss about this he said we would never design our own joists for a client, we would just assign proper loads for someone like Vulcraft to meet our specifications. The reason I want to learn to do this is that this summer, for my masters program, I will be taking Advanced Strength of Materials and Advanced Structural Analysis. For both these classes we must do a project. I would like to make this one of my projects. However, with my checks on my progress so far I certainly feel their are many other checks I am missing. Any guidance is appreciated.
Thanks,
For a K series joist I want to use the following:
Top Chord: Double Angles (Equal lengths)36 Ksi
Web: Single Angle (Uncrimped-First analysis, Crimped-Second Analysis)36 Ksi
Bottom Chord: Double Angles (Equal lengths) 36 KSI
Rods at each ends from bottom chord to top chord.
The Vulcraft Manual states the bottom chord to be checked in axial tension only, web in compression, and top chord in axial compression ONLY if panels are less than 24" apart.
I've used Chapters D,E,and F.
D2
E3 & E4
F9
When I asked my boss about this he said we would never design our own joists for a client, we would just assign proper loads for someone like Vulcraft to meet our specifications. The reason I want to learn to do this is that this summer, for my masters program, I will be taking Advanced Strength of Materials and Advanced Structural Analysis. For both these classes we must do a project. I would like to make this one of my projects. However, with my checks on my progress so far I certainly feel their are many other checks I am missing. Any guidance is appreciated.
Thanks,