Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SSS148 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Static dissipative plastic used for fixturing ESD sensitive components

Status
Not open for further replies.

chopper75

Aerospace
Sep 27, 2011
95
I would like to use a 3D printed tray to hold SMT components that are ESD sensitive. The 3D printed material has the following specs and I'm wondering if it will be safe to use:

Volume resistivity: 3.2 x 10exp11 ohm-cm
Surface Resistivity: 3.2 x 10exp11 ohm
dissipation Factor, 1 KHz: .177
Dielectric Constant, 1 KHz: 6.27
Dielectric Strength: 221kV/in

 
Replies continue below

Recommended for you

There are conductive paints that should work to prevent static buildup.
 