I am looking at the intensity of erosion generated by the jet of steam and condensate released when a steam trap opens.

Is anyone aware of any test data or calculation methods for estimating -

1. The velocity of steam jets generated by condesnate depressurising through a small orifice

2. The flow rate of by condesnate depressurising through a small orifice

3. Methods of estimating the erosion rates of SG iron or different steels caused by droplet or caviation erosion?

Thanks for your help.

Neil
 
Replies continue below

Recommended for you

Probably a company that manufactures steam traps, like Armstrong, Spirax Sarco etc would have this info. If you can use a trap with a dribble discharge, like a float & thermostatic, it will greatly reduce the erosion. Otherwise, it's pretty much put a heavy 90* el immediately after the trap, let it take the blast, and periodically replace it.
 