ajk1
Structural
- Apr 22, 2011
- 1,791
Given the chemical composition of the steel as determined form specimens cut form existing rebar from an old building, how is the weldability determined?
What is the formula, and what is the criteria for assessing its weldability?
Is the formula for wledability as follows:
%C + %Mn/6 + %Ni/20 +%Cr/10
correct, and if so, what is the acceptance criteria? If this is not the correct formula, what is?
A representative specimen is as follows:
Carbon 0.39?
Manganese 0.66%
Chromium 0.04%
Nickel 0.04%
What is the formula, and what is the criteria for assessing its weldability?
Is the formula for wledability as follows:
%C + %Mn/6 + %Ni/20 +%Cr/10
correct, and if so, what is the acceptance criteria? If this is not the correct formula, what is?
A representative specimen is as follows:
Carbon 0.39?
Manganese 0.66%
Chromium 0.04%
Nickel 0.04%