287
I noticed that one specification for a slide valve in a product coke line of a fluid coker it was recommended that the hardfacing be made of Stellite 6 followed by Stellite 1. Why do you suppose that was recommended?

Also, does anyone have experience with the carburization resistance of Stellite? Operating temperature is close to 1100 F.
 
Replies continue below

Recommended for you

I have seen intermediate layers used for overlay, but 6 is so hard to start with I don't know why you would use it.
The high Co alloys have very good resistance to Carb.

= = = = = = = = = = = = = = = = = = = =
Rust never sleeps
Neither should your protection
 