Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Stiffness defined by engineering constants is not physically reasonable?

Status
Not open for further replies.

IcarusAero223

Aerospace
Mar 10, 2024
10
I calculated equivalent elastic properties of a honeycomb core using analytical Ashby & Gibson approach.
Material was defined using "Engineering Constants" submenu in elastic material properties section (with analitically calculated values).
After that I defined material orientation using local datum CSYS.

But running the simulation, an error occurs saying: "Stiffness defined by engineering constants is not physically reasonable. Check choice of poisson's ratios. Stiffness defined by engineering constants is not physically reasonable. The total work done by all strain components must be positive. Check choice of poisson's ratios".

I did an orthotropic stability condition check and none of the conditions were met. Then I did the same check for values found in other literature and there those conditions weren't met either.

Any help is greatly appreciated, THANKS!

Part geometry with local datum CSYS

Material properties window
 
Replies continue below

Recommended for you

IcarusAero223 said:
Then I did the same check for values found in other literature and there those conditions weren't met either.

And are they accepted by Abaqus ? Check with the data provided for the examples in the Abaqus documentation.
 