GeauxTiger10
Structural
- Feb 2, 2011
- 1
Looking for the maximum spacing requirements for stirrups in 24” deep grade beams. The stirrups would be used to hold the rebar in place, essentially as ties for the reinforcement as they would not be required for shear. I’m thinking 48” O.C. would be sufficient, but are there any other codes pertaining to maximum stirrup spacing?
ACI 318 Section 11.5.4 provides stirrup spacing requirements for shear; however, minimal shear is occuring.
IBC 2006 refers to ACI 318.
WRI: Design of Slab-on-Ground Foundations states “FOR BEAMS 36” TO 54” DEEP USE #3 STIRRUPS AT MAXIMUM 24” O.C.”
ACI 318 Section 11.5.4 provides stirrup spacing requirements for shear; however, minimal shear is occuring.
IBC 2006 refers to ACI 318.
WRI: Design of Slab-on-Ground Foundations states “FOR BEAMS 36” TO 54” DEEP USE #3 STIRRUPS AT MAXIMUM 24” O.C.”