Mohamedsayed
Civil/Environmental
- Apr 16, 2013
- 61
Hello
I am working on a material whose stress strain curve is strain hardening (concave upward), unlike the steel whose strain harening is concave downward.
the problem is when i calculate the equivalent plastic strain, it is negative. the following table represents the true stress-strain curve for the material that i am talking about.
0 0
143.4108527 0.1
405.1094891 0.2
637.9310345 0.25
768.8558235 0.27
1034.161491 0.3
1149.298597 0.31
1485 0.33250487
and this table represents the yield stress vs. Abs.plastic strain.
142.1994 0
169.8456962 -0.004242229
273.8821714 -0.032129522
445.4397035 -0.101488562
661.5232314 -0.208943057
912.2319088 -0.351022659
1183.168317 -0.515740219
1469.77675 -0.699728928
1485 -0.70950104
When i do that, i got error message that the value should be in ascending order.
Do you know how can i solve that problem.
Thanks
I am working on a material whose stress strain curve is strain hardening (concave upward), unlike the steel whose strain harening is concave downward.
the problem is when i calculate the equivalent plastic strain, it is negative. the following table represents the true stress-strain curve for the material that i am talking about.
0 0
143.4108527 0.1
405.1094891 0.2
637.9310345 0.25
768.8558235 0.27
1034.161491 0.3
1149.298597 0.31
1485 0.33250487
and this table represents the yield stress vs. Abs.plastic strain.
142.1994 0
169.8456962 -0.004242229
273.8821714 -0.032129522
445.4397035 -0.101488562
661.5232314 -0.208943057
912.2319088 -0.351022659
1183.168317 -0.515740219
1469.77675 -0.699728928
1485 -0.70950104
When i do that, i got error message that the value should be in ascending order.
Do you know how can i solve that problem.