Is anyone aware of timber grading systems for small section timbers - 50x50mm (2"X2") or less? These fall outside the usual C16, C24 system I am used to in the UK/EU. Maybe for non-structural contexts?

Reason: client wants a geodesic greenhouse in timber.
 
Replies continue below

Recommended for you

Interestingly, clear wood specimens are tested at that size, per ASTM D143.

SPIB’s National Grading Rule allows for 2-inch by 2-inch but no smaller.
 
Our code has "No1 framing" grade which is basically ungraded landscaping timber I think
You may have some equivalent?
 
Would any fasteners have enough pullout capacity needed for lateral or uplift wind forces, plus the potential of fasteners splitting the 2x2 lumber?
 
Would any fasteners have enough pullout capacity needed for lateral or uplift wind forces, plus the potential of fasteners splitting the 2x2 lumber?
This is the next question! In principle edge distance are sufficient for small screws/nails at 45mm but...
 
yea, I can't imagine getting fasteners to work for this unless you had some sort of receivers they frame into
 
Because screws have a tendency to split the wood, even predrilled. Bolts can be torqued down to give a tight connection (use large washers), and a solid shank bolt is stronger in shear than a threaded screw.
 
Because screws have a tendency to split the wood, even predrilled. Bolts can be torqued down to give a tight connection (use large washers), and a solid shank bolt is stronger in shear than a threaded screw.
Precisely because of wood’s propensity to split, the traditional design philosophy is to use more, smaller fasteners. I would never use a bolt on something this small.
 
I will second ANE91 here, despite edge distance requirements are less 4*D for bolts vs 5*D (in Aus) for screws in shear perp grain, bolts are way more in diameter. I will be spec-ing them a metal strap if edge distance cant be met, we can have an idea of tendency to split using following reference in AS1720.1 (or any alternative ref to your locality)