see attached...i have a bracket w/1500 psi of pressure hitting the point shown
it is held in place with the static pin also as shown
we need this bracket to deform slightly yet not "bend" out of shape.
the bracket is .730" thick...everything is in inches
as of right now this thing does not budge...the question is what do i need to change .395 to, in order
for this bracket to deform while installing yet not pass the modulus of elasticity?
i don't expect a sure fire answer here, just a direction or software, a formula....something to get
this off the ground...material is 304ss by the way
thank you in advance
see attached...i have a bracket w/1500 psi of pressure hitting the point shown
it is held in place with the static pin also as shown
we need this bracket to deform slightly yet not "bend" out of shape.
the bracket is .730" thick...everything is in inches
as of right now this thing does not budge...the question is what do i need to change .395 to, in order
for this bracket to deform while installing yet not pass the modulus of elasticity?
i don't expect a sure fire answer here, just a direction or software, a formula....something to get
this off the ground...material is 304ss by the way