andrewleong
Mechanical
- Feb 8, 2012
- 7
Does a stainless steel flush-type clean out fitting requires thermal stress relief?
According to clause 5.7.4.1, all flush-type clean out fitting require thermal stress relief.
While Appendix D section 3.7 - 650-I-33/99 also states that stress relief is required regardless of the material used.
However under Appendix S, clause S.3.3.2 indicates that thermal stress relief requirements of 5.7.4 are not applicable for stainless steel.
Could anyone clarify on the above?
Many thanks.
According to clause 5.7.4.1, all flush-type clean out fitting require thermal stress relief.
While Appendix D section 3.7 - 650-I-33/99 also states that stress relief is required regardless of the material used.
However under Appendix S, clause S.3.3.2 indicates that thermal stress relief requirements of 5.7.4 are not applicable for stainless steel.
Could anyone clarify on the above?
Many thanks.