1
I have a superheat manufactured with 27 mm,2.9mm wall thickness tube of grate 211-T 111.

After manufacturing,should i stress relieve this ….if yes, at what temperatures to prevent and distortion of bend.
 
Replies continue below

Recommended for you

What exactly is the material? Code of construction?
 
Further Information on Mr Suhail's question:

Material: Alloy Steel Seamless Tube (SA213 T11) Dia 31.8mm x 3mm w.t.
Job: Replacement of Superheater Tubes
Construction Code: ASME Sec 1/ ASME B31.1 (Power Piping)
 
In this case, no PWHT is necessary based on wall thickness.
 