I have a question about stud bolt of high speed impeller rotor.
Actually we have high speed compressor (about 40000rpm) in our plant. After some year we change impeller due high erosion, with new one.
We know amount of impeller torque of stud and because of high defection, it's tight and uptight many time (about 3 or 4 time). Is this stud bolt design just for one time use or we had to replace it each time with change of impeller?
Thanks
I have a question about stud bolt of high speed impeller rotor.
Actually we have high speed compressor (about 40000rpm) in our plant. After some year we change impeller due high erosion, with new one.
We know amount of impeller torque of stud and because of high defection, it's tight and uptight many time (about 3 or 4 time). Is this stud bolt design just for one time use or we had to replace it each time with change of impeller?