Thank you so much for the replies I got.
I think I found out the calculation and it is the result I have.
Initial oil temp = 250F
Length of pipeline = 25km
Insulation material = polyurethane (k=0.025)
Surrounding temp (temp sea water) = 39F
I get the final temp at around 125F with 1in thick insulation. Could someone verify this please? It just sounds like too good to be true.
I am new to this industry and I don't have any previous project that I can compare this against.
Thanks!
I think I found out the calculation and it is the result I have.
Initial oil temp = 250F
Length of pipeline = 25km
Insulation material = polyurethane (k=0.025)
Surrounding temp (temp sea water) = 39F
I get the final temp at around 125F with 1in thick insulation. Could someone verify this please? It just sounds like too good to be true.
I am new to this industry and I don't have any previous project that I can compare this against.
Thanks!