I am trying to bond a layer of ABS ( smooth on one side, haircell or 'orange peel' on the other; can bond to either side ) to a flat piece of smooth pine wood. The bonded parts will not undergo great forces, but will need to last and withstand minor shear forces. ( I don't have quantitative estimates of what forces are involved )

I am going to try:
- some kind of epoxy
- silicon
- wood glue ( yikes! )

Am I crazy?
Any other ideas of what to try or specifics on those mentioned above?

Thanks for any advice.

Cheers,
DHD
 
Replies continue below

Recommended for you

A friend built some cases for his music instruments recently, and used contact cement, like you would use for floor tiles or vinyl flooring material, to bond abs to plywood.
 
Interesting. I'll give that a go too.

So far I've tried a gel epoxy, silicone, and wood glue.

The wood glue held up horribly. No surprise.
The epoxy held up to a moderate 'peeling' force, but somewhat gave way to vigorous peeling.
The silicone sealant has held up well to any kind of 'peeling' force I've tried.