I will manufacture Tees, Elbows and Crosses, austenitic stainless steel grade 316/316L - Closed die forgings.
My client's specification requests a control of the "Sulphur" element (0.005-0.012%).
Why do you have this sulfur control? Is it because the material is open die forged?