Dear Readers,

1. Does anyone know, how long is a sulphur plant using superclaus claus process can operate continuously at best? We have sulphur plant but its reliability is terrible. Our best record was only 5 months continuous operation. There a lot of modification and material upgrading have been done but not helping much.

2. One of our problem is H2S/SO2 analyser plugging every 3 days. Does anyone have similar problem? What sort of effort have been done to solve this problem?

Thank you for your help
 