mechengineer
Mechanical
- Apr 19, 2001
- 268
Dear experts,
The super duplex 24" elbow (SA-815) will be made by plate. Question: are there any limits from a code/standard for using two weld lines on the elbow, the half welds to the half? The user wants a single weld seam, but the vendor wants to use double seams for the 24" elbow. It is not mentioned clearly in the contract.
Thanks
The super duplex 24" elbow (SA-815) will be made by plate. Question: are there any limits from a code/standard for using two weld lines on the elbow, the half welds to the half? The user wants a single weld seam, but the vendor wants to use double seams for the 24" elbow. It is not mentioned clearly in the contract.
Thanks