hello everyone i am new here and this is my first topic
i'm a QC supervisor and we have a problem with some saddle support for a heat recuperator duct with 4100 mm Diameter,
the main problem is the saddle are no in 100% contact with the duct , they have a gap like 5-7 mm, in a 70% of the saddle lenght but i need to support with a code or specification that saddle need to be in touch in the 100% of the section. the fabricacion of the duct was in italy but installed in mexico.
the duct is only for air, and they only support his own weight, i am not sure if 100% is necessary, actually it in contact in the edge saddles
i'm a QC supervisor and we have a problem with some saddle support for a heat recuperator duct with 4100 mm Diameter,
the main problem is the saddle are no in 100% contact with the duct , they have a gap like 5-7 mm, in a 70% of the saddle lenght but i need to support with a code or specification that saddle need to be in touch in the 100% of the section. the fabricacion of the duct was in italy but installed in mexico.
the duct is only for air, and they only support his own weight, i am not sure if 100% is necessary, actually it in contact in the edge saddles