Surface finish 1

Status
Not open for further replies.

lurks

Mechanical
Sep 18, 2007
83
Does anybody know if there is an ASTM spec for the surface finish of cold formed steel?

Thanks,

lurks
 
Replies continue below

Recommended for you

I normally see finish called out for stainless steel sheet. ASTM A 480 covers sheet finish for flat rolled stainless and heat resisting steel plate, sheet and strip. It applies to ASTM A 167, A176, A 240, A 263, A 264, A 265, A 666, A 693, A 793, and A 895.

This not an RA surface finish specification like ASME B 46.1. Instead, section 11 describes the finish for sheet as follows:
11.1 The types of finish available on sheet products are:
11.1.1 No. 1 Finish—Hot-rolled, annealed, and descaled.
11.1.2 No. 2D Finish—Cold-rolled, dull finish.
11.1.3 No. 2B Finish—Cold-rolled, bright finish.
11.1.3.1 Bright Annealed Finish—A bright cold-rolled finish retained by final annealing in a controlled atmosphere furnace.
11.1.4 No. 3 Finish—Intermediate polished finish, one or both sides.
11.1.5 No. 4 Finish—General purpose polished finish, one or both sides.
11.1.6 No. 6 Finish—Dull satin finish, Tampico brushed, one or both sides.
11.1.7 No. 7 Finish—High luster finish.
11.1.8 No. 8 Finish—Mirror finish.
11.1.9 TR Finish—Cold-worked to obtain specified properties.
NOTE 4—Explanation of Sheet Finishes:
No. 1—Commonly referred to as hot-rolled annealed and pickled or descaled. This is a dull, no reflective finish.
 
fabrication codes may also have requirements for surface roughness.
 