Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

surface resistivity

Status
Not open for further replies.

dho

Mechanical
May 19, 2006
255
i am hit by a requirement, the surface resistivity.
to prevent any electrical energy stored on the surface, the surface resistivity must be between 1 megohm per square and 100 megohm per square.
my unit are made from anodized aluminum. i searched the internet for a number and could not find one.
is there a published document on such information?
thanks.
 
Replies continue below

Recommended for you

First off, what grade & type of anodize

For instance 'Hard Anodize' is thicker and more resistive than some other types.

Not saying you can trust it in isolation but a quick Google search got me:

Posting guidelines faq731-376 (probably not aimed specifically at you)
What is Engineering anyway: faq1088-1484
 
Unless they are measuring based on thickness of anodize layer?

Posting guidelines faq731-376 (probably not aimed specifically at you)
What is Engineering anyway: faq1088-1484
 
i will think the thickness of the anodize layer may impact the surface resistivity, but by definition, the unit should be ohm per square.
so, that article either not valid or needs correction.
not too much info online. [sad]
 
It's very well explained here:
TTFN
faq731-376
7ofakss

Need help writing a question or understanding a reply? forum1529


Of course I can. I can do anything. I can do absolutely anything. I'm an expert!
There is a homework forum hosted by engineering.com:
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor