Dear Expertise,
We are in final process to order a water tube boiler with 125 T/h capacity. The vendor is insisting to use swaged tubes for the connection between the tubes and mud drum. Our specifications is not allowing for that. Can you please tell me the advantage and disadvantage to use the swaged tubes?
Thanks for your valuable support.
We are in final process to order a water tube boiler with 125 T/h capacity. The vendor is insisting to use swaged tubes for the connection between the tubes and mud drum. Our specifications is not allowing for that. Can you please tell me the advantage and disadvantage to use the swaged tubes?
Thanks for your valuable support.