MGMech
Mechanical
- Apr 2, 2015
- 10
Hi,
We are designing new Cabin Say Bar (Stabilizer bar or Anti-roll bar). I am searching information for material selection for good fatigue properties and also good weldability, proper heat treatment, optimum welding parameters. It seems quite big job to me.
We will use hollow tube, it is welded to forged steel at both ends. material alterantives seem 34MnB5, 26MnB5, AISI 4140(42CrMo4), AISI 4130 (25CrMo4). I haven't seen any other alternatives than these ones. Austenize temperature and quenching time can not be optimized because our supplier always make the same process. Austizeing is done between 900-1000 Celciues degree, quenching is done at oil. We can only optimize tempering temperature. I want to test weldability and fatigue performance of sway tubes those are tempered at three different tempering temperatures. I do not know if it will worth to check different tempering temperatures.
I am not sure for Forged metal at ends. I think welding to forge metal is better than welding to cast iron but I could not find good information to provide. And I think it would be better if sway tube material matches with forged steel. So, I am close to select 4140 forged steel.
I need to prepare welding and fatigue properties with GMAW (MIG) Welding. For serial production, Magnetic Impelled Arc Welding is best however machines are very expensive like 1 million dollar. So it is also possible to make GMAW at serial production.
It seems like opmization problem between welding and best fatigue performance. I will be happy if you can help me.
We are designing new Cabin Say Bar (Stabilizer bar or Anti-roll bar). I am searching information for material selection for good fatigue properties and also good weldability, proper heat treatment, optimum welding parameters. It seems quite big job to me.
We will use hollow tube, it is welded to forged steel at both ends. material alterantives seem 34MnB5, 26MnB5, AISI 4140(42CrMo4), AISI 4130 (25CrMo4). I haven't seen any other alternatives than these ones. Austenize temperature and quenching time can not be optimized because our supplier always make the same process. Austizeing is done between 900-1000 Celciues degree, quenching is done at oil. We can only optimize tempering temperature. I want to test weldability and fatigue performance of sway tubes those are tempered at three different tempering temperatures. I do not know if it will worth to check different tempering temperatures.
I am not sure for Forged metal at ends. I think welding to forge metal is better than welding to cast iron but I could not find good information to provide. And I think it would be better if sway tube material matches with forged steel. So, I am close to select 4140 forged steel.
I need to prepare welding and fatigue properties with GMAW (MIG) Welding. For serial production, Magnetic Impelled Arc Welding is best however machines are very expensive like 1 million dollar. So it is also possible to make GMAW at serial production.
It seems like opmization problem between welding and best fatigue performance. I will be happy if you can help me.