Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations GregLocock on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Tank floor plate differences on replacement

Status
Not open for further replies.

Tanks to you

Petroleum
Oct 1, 2021
2
Does anyone know if there is a limit on mismatched floor plates? ie 5/16" to 3/8". I know there is a restriction on shells but can't quite find anything on floor plates.

thanks in advance
 
Replies continue below

Recommended for you

For API 650 tanks with fully supported bottoms, it's quite common to use 3/8" annular plates and 5/16" bottom plates. As long as you are above the API minimum you should be OK, unless there is a specific reason for the thicker material that the thinner material can't handle. My opinion only...remember - you read it on the World Wild Web
 
True enough and thanks. I guess my question is more of a floor plate mismatch. ie a bottom floor needs a plate replaced and all that is available is the thicker material.
 
Status
Not open for further replies.