Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Temperature limit of sheroidal graphite cast iron valves and PED certification 1

Status
Not open for further replies.

fabiobs

Industrial
Joined
Jan 18, 2016
Messages
10
Location
IT
Hello,
I have a simple question.
I know that many valves (gate, butterfly...) are casted in spheroidal graphite GJS 400-15 that is limited to -10°C but in the data sheet and PED certificate are marked up to -20°C. How is it possible?
 
I am afraid you will have to give the exact details (datasheet for the valve and regulation/text) before you will get an answer.

 
Many regulation like EN 12516-4 or EN 15776 indicate as low temperature limit for GJS 400-15 or GJS 450-10 -10°C. Many manufacturers of butterfly and gates valves indicate as low temperature limit -20°C. In Europe there is PED (pressure equipment directive) and use of material below the temperature indicated in the regulation must be justified. My question is easy: how can be use a casted spheroidal graphite below temperature limit?
 