Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SSS148 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Temperature rating of SA 516 Gr 60 3

Status
Not open for further replies.

Moossii

Chemical
Dec 27, 2017
4
Hello,
Where should I look to find out the minimum temperature rating of SA 516 Gr 60?
 
Replies continue below

Recommended for you

Yes sir. The ASTM equivalent is A 516 Gr 60
 
If you mean the lowest permitted temperature that will depend on material thickness and heat treatment in ASME Section VIII, Div 1.
 
See UCS-66. Look at the curves in the figure therein.
 