Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Tek-Tips community for having the most helpful posts in the forums last week. Way to Go!

Tensile and flexural modulus

Status
Not open for further replies.

APH

Mechanical
Sep 7, 2004
79
0
0
US
What is the different between the two and where they are used respectively.

Thanks
APH
 
Replies continue below

Recommended for you

Flexural Modulus: The ratio, within the elastic limit, of the applied stress on a test sample in flexure to the corresponding strain in the outermost fibers of the sample.

Tensile Modulus: The measure of the initial resistance of a material to longitudinal stretching.


 
Hai APH,

Flexural modulus applies to bending.
Tensile modulus applies to stretching mentioned by Miner00 and allen4 is right

Usually for metals, Flexural modulus = Tensile modulus.

But for plastics flexural modulus is quiet different from tensile modulus as well as compressive modulus.You can check it out at
Regards,