Table J2.5 of AISC 360-05, Fillet Welds Section, Tension or Compression parallel to a weld axis states: Tension or compression in parts joined parallel to a weld need not be considered in design of welds joining the parts. Graphically, what does this mean?
To simplify, let's say I have a cantilevered flat bar, 3"x1/2", long dimension vertical, with fillet welds along each 3" face. Ignore the length of the cantilever. At the end of the bar I have a vertical load acting down and a lateral tension load pulling away from the host support.
Typically, I'll resolve the vertical load into a y-component stress, y1. Next I'll find the moment induced tension on the weld and calculate the x-component stress at the furthest distance from my centroid, x1. Next I'll find the additional x-component stress from the tension load alone, x2. Resolving these forces [(y1)² + (x1+x2)²]0.5 = the resolved stress on my weld. This will be used to size the weld, etc. (For the record, as you can see, I'm using an elastic vector analysis)
At what point can I ignore the tension or compression stress as mentioned in Table J2.5? Is this ONLY when there is a tension force, and no other force that is inducing shear through the axis of the weld?
To simplify, let's say I have a cantilevered flat bar, 3"x1/2", long dimension vertical, with fillet welds along each 3" face. Ignore the length of the cantilever. At the end of the bar I have a vertical load acting down and a lateral tension load pulling away from the host support.
Typically, I'll resolve the vertical load into a y-component stress, y1. Next I'll find the moment induced tension on the weld and calculate the x-component stress at the furthest distance from my centroid, x1. Next I'll find the additional x-component stress from the tension load alone, x2. Resolving these forces [(y1)² + (x1+x2)²]0.5 = the resolved stress on my weld. This will be used to size the weld, etc. (For the record, as you can see, I'm using an elastic vector analysis)
At what point can I ignore the tension or compression stress as mentioned in Table J2.5? Is this ONLY when there is a tension force, and no other force that is inducing shear through the axis of the weld?