Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations 3DDave on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

tension strength for concrete

Status
Not open for further replies.

robyengIT

Mechanical
Dec 20, 2013
894
as far as You know, there is any literature about relation between tensile (not compressive) strength of concrete directly found in lab (with proper specimen) and the tensile strength indirectly found in lab with the cylinder specimen (brazilian test) ? Usually the standard provides a formula stating the tensile strength from the failure load of the brazilian test
Thanks
 
Replies continue below

Recommended for you

To my knowledge, there is no credible direct tension test for concrete. This is because there are many variables that affect concrete tensile tests. For instance, even a slight variation in distribution of the coarse aggregate in the concrete will change its tensile properties but not affect its compression properties.

The two common tests are splitting tensile and flexural tests. It is easy to do a correlation between splitting tensile and flexural as you can use the same specimen for both tests.

Here is a link to some additional information.....

Concrete Testing


A Great Place For Engineers to Help Engineers

Follow me there.....
 
Here is some literature that may feed your quest.

Report DSO-2018-11 "Developments for the Concrete Tensile Split Test" - Dam Safety Technology Development Program Link

Report DSO-2016-02 "Concrete Tensile Strength Specimen Size Effects" - Dam Safety Technology Development Program Link

Publication Number: FHWA-HRT-06-103 Date: August 2006
"Material Property Characterization of Ultra-High Performance Concrete" Link
 