gluca
Petroleum
- Sep 23, 2006
- 9
Talking about tensile tests according to ASTM A234 WPB; if I make a butt welding fitting starting from a plate with wall tickness 25 mm, I have to normalize (heat treatment) this fitting. Very often the plates are furnished as rolled, not heat treated, but the tensile tests reported on the 3.1 certificate (of the starting plate) are performed on normalized samples of these plates.
Do I have to perform new tensile tests for my normalized fitting, or can I use the records of the test on the starting plate to declare that the fitting meet the ASTM A234 tensile requirements. The starting plate was not heat treated, but the samples have been heat treated in the same manner as my fitting.... Thanks, Gianluca
Do I have to perform new tensile tests for my normalized fitting, or can I use the records of the test on the starting plate to declare that the fitting meet the ASTM A234 tensile requirements. The starting plate was not heat treated, but the samples have been heat treated in the same manner as my fitting.... Thanks, Gianluca