Hiya everyone,
I was just wondering if anybody knows how I can test for the presence of aluminium oxide? We have been shot blasting plastic with an aluminium oxide abrasive, so bits of this abrasive will be left on the surface of the plastic. We believe that we can remove this aluminium oxide using acetic acid (white vinegar). However, it is essential that there is no aluminium oxide left on the surface of the plastic. We therefore need some way to test for this.
Thanks
Kat
I was just wondering if anybody knows how I can test for the presence of aluminium oxide? We have been shot blasting plastic with an aluminium oxide abrasive, so bits of this abrasive will be left on the surface of the plastic. We believe that we can remove this aluminium oxide using acetic acid (white vinegar). However, it is essential that there is no aluminium oxide left on the surface of the plastic. We therefore need some way to test for this.
Thanks
Kat