The manufacterer of the stripper ov

Status
Not open for further replies.

ENGRANIA

Mechanical
Dec 17, 2008
34
The manufacterer of the stripper overhead accumulator has choosen the material of shell and head astm a- 387 gr22 cladding with monel although a-387 is good at elevated pressure and temperature . I don't know what the reason of using cladding for monel.
 
Replies continue below

Recommended for you

Monel would prevent corrosion due to condensation, which is basically acidic corrosion.

DHURJATI SEN
Kolkata, India


 
Cladding is a way to get the high corrosion resistance at a lower cost

--- Best regards, Morten Andersen
 
You are welcome,..... ENGRANIA

MJCronin
Sr. Process Engineer
 
@ENGRANIA
"stripper overhead accumulator" - what does this stripper strip and what does this accumulator accumulate?
 
Engrantia

Monel cladding is for corrosion purposes, but in what service will be aplicated the stripper overhead vessel?

regards

luis
 