I am looking for a adheasive that wil bond my activated cabon particles to a metal substrate that will not wick up through the pores in the carbon. Any sugestions will be appreciated.
The first link is to graphite based adhesives. The second
link is to EMS that have a good cross section of various
adhesives. The third link is to Epo-Tek maker of a lot of the
adhesives in the EMS list.