I'am working on a thermo-mechanical(explicit) model using the step Dynamic, temp-disp, explicit,I have two discrete rigid parts with a deformable part ( dies and a workpiece) because i'am modelling a hot forging model.
- Interactions : surface to surface contact / surface film condition
- system units: mm/s/mJ/T/MPA
- Mesh : C3D8RT for the workpiece,hex and structured elements
- BC : Velocity for the top die and the bottom die is encastred
- Predefined field : each part has its initial temperature of forging
- interaction property : Normal / tangential / thermal conductance
- properties: density, elastic plastic,conductivity and heat capacity ( temperature-dependent data)
My question is why do i always have such a problem ( see picture joined here) ? even when i refined the mesh, the problem seemed to occur again and again. Another problem is that with the mesh refinemend my problem takes tooo much time for the calculcation, really too many increments, for 1 sec time period , my laptop spent two days to be at 0.25 s !! What can be the cause please ? is it due to the complexity of the model ? or is it related to my laptop performances ? i have an intel core i7 processor( 2 cores) but a good graphic card ( NVIDIA quadro k2100M) and a 16 GB RAM ! if there is any adjustment to do in order to accelerate the calculation, i will be glad !!
PS : for more enlightment i can send the cae model by e-mail to make thigs more clear.
I'am working on a thermo-mechanical(explicit) model using the step Dynamic, temp-disp, explicit,I have two discrete rigid parts with a deformable part ( dies and a workpiece) because i'am modelling a hot forging model.
- Interactions : surface to surface contact / surface film condition
- system units: mm/s/mJ/T/MPA
- Mesh : C3D8RT for the workpiece,hex and structured elements
- BC : Velocity for the top die and the bottom die is encastred
- Predefined field : each part has its initial temperature of forging
- interaction property : Normal / tangential / thermal conductance
- properties: density, elastic plastic,conductivity and heat capacity ( temperature-dependent data)
My question is why do i always have such a problem ( see picture joined here) ? even when i refined the mesh, the problem seemed to occur again and again. Another problem is that with the mesh refinemend my problem takes tooo much time for the calculcation, really too many increments, for 1 sec time period , my laptop spent two days to be at 0.25 s !! What can be the cause please ? is it due to the complexity of the model ? or is it related to my laptop performances ? i have an intel core i7 processor( 2 cores) but a good graphic card ( NVIDIA quadro k2100M) and a 16 GB RAM ! if there is any adjustment to do in order to accelerate the calculation, i will be glad !!
PS : for more enlightment i can send the cae model by e-mail to make thigs more clear.