marcFACT
Materials
- Aug 1, 2016
- 3
Hi All,
I'm looking for a way to check the thickness of large pieces of honeycomb (1500mmx1500mm)
Until now we've been measuring the thickness at various points along the edges and averaging out, however this is not very accurate as it doesn't take any measure of the points within the edges.
Our process is very thickness sensitive and there seems to be a considerable amount of variation coming from our suppliers.
Ideally I would like a method to ensure the majority of the honeycomb piece is NOT LESS than X mm, with a precision of at least 0.05mm
Are there any standard methods of making this kind of dimensional check?
Thanks for your help!
I'm looking for a way to check the thickness of large pieces of honeycomb (1500mmx1500mm)
Until now we've been measuring the thickness at various points along the edges and averaging out, however this is not very accurate as it doesn't take any measure of the points within the edges.
Our process is very thickness sensitive and there seems to be a considerable amount of variation coming from our suppliers.
Ideally I would like a method to ensure the majority of the honeycomb piece is NOT LESS than X mm, with a precision of at least 0.05mm
Are there any standard methods of making this kind of dimensional check?
Thanks for your help!