Notes from email with a picture. I believe these parts were made in Mexico.
The thread
is not well manufactured(attached photo) but when using the gauge it enters correctly, can it be approved. (600 pieces).
I looked at this picture and it looks like a straight thread but it's a 1" NPT that gaged to L1. I think because it uses Teflon tape to seal or sealant, the crests aren't so critical. I'm not sure what to check other thn to ask them to make one up to a test plug and pressure test using 4 turns past finger tight.
Thoughts?
The thread
is not well manufactured(attached photo) but when using the gauge it enters correctly, can it be approved. (600 pieces).
I looked at this picture and it looks like a straight thread but it's a 1" NPT that gaged to L1. I think because it uses Teflon tape to seal or sealant, the crests aren't so critical. I'm not sure what to check other thn to ask them to make one up to a test plug and pressure test using 4 turns past finger tight.