Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Threaded TEE for 9 5/8" casing 1

Status
Not open for further replies.

jorgerobles

Mechanical
Jan 14, 2004
5
Hello, for an experimental setup I need to connect a 6in pipe line to a 9 5/8” casing. I wonder if there is any kind of standard piece that I could use (or modify to be used) as a tee.
Thanks,
JR
 
Replies continue below

Recommended for you

What ever way you look at it you will need a tee, you can use butt weld tees, this is a non stock item but can be manufacturers just find a graded fitter (G6 standard) API and have them prefab it for you. they will need to know the cold working pressure (CWP) and the test pressure

The CWP is the pressure you expect to be running through the pipes

You can then add or cut threads or if it is to be permanent weld
 