csd72

Structural
May 4, 2006
4,574
I have a through plate slotted through the center of a 6x6 tube.

Looking up the AISC Hollow structural Connections manual they say to treat it the same as a face welded gusset, even for bending of the face.

The thing that I cant understand is that now I have a slot cut out of the face of the tube and only a fillet weld to connect it. How can this be taken as the same as a continuous face? Am I missing something?
 
Replies continue below

Recommended for you

Two seperate cantilevers off the tube corners perhaps?

 
You have two filets, one on each side to replace the continuous face. It becomes continuous by continuous connecting parts.
 
JAE,

yes I thought of this. P/2XL/2 = PL/4 same as for the span, but the design method uses a width morethan the plate.

civilperson,

The weld has to be quite large to make this work (1/2" fillet weld in my case) which is far heavier than the design method would require.

Thanks for the help. I ended up using a T bracket welded to the webs. This gives me a more predictable result.
 