tig welding tubing, fitting face perpendicular to tubing

Spike2000

Mechanical
Sep 12, 2012
19
looking for some existing fixturing or ideas on how to hold a very tight tolerance on butt welding a 4" fitting to 4" o.d. tubing with a perpendicular tolerance of .015"
we are tig welding and our current tolerance is .032" on this dimension, thank you in advance
 
Replies continue below

Recommended for you

OP
Is this only one or or high volume.


Buy a tool cast plate large enough to hold assembly.
Buy soft angle plate.
Draw out the birds eye view of the layout
Obtain dimensions to assemble and weld
Assembly. Generally due to weld shrink and slight distortion it's generally best to fitup and weld inner assembly and cut and fit up flanges last. All angle flanges must be secure to the cast plate , socket head bolts or equivalent.
Mill out angle flanges with cradles to hold assembly during fitting and welding.
Drill out holes to bolt flanges when welding.
Angle flanges must be precision machined.
Faces perpendicular and square.
 
Last edited:
Thank you for the response, 2-3 pcs for prototype then production run quantities...100's of pcs
 
Are you using automated orbital welding?
If you are doing this by hand are you using a rotator to control the speed?
Are you welding in sections as opposed to 'all the way around in one shot?
If you really want to hold 0.015" your original fit will need to be <0.005" out.
 
semi auto welding, one shot
less than <.005" out....yikes

thank you
 
OP
Actually welding fixture is for tacking , then weld .
It's critical to work from inside, then do the flanges last while it is restrained. Cut to fit up then tack. Then weld. While restrain.
 