Tin silver alloy question.

Status
Not open for further replies.

janeriksen

Industrial
Jan 15, 2011
25
Tin silver alloy is a very soft metal, but is it possible to mix another metal into it in order to get a golden color without hardening it too much?
 
Replies continue below

Recommended for you

What is the 'gold' colored alloy that they used for tableware?
There are some Cu based alloys that are very yellow (not orange).
I'll bet that the CDA has literature on the colors of various alloys.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
I use a silver brazing alloy that has a gold tint. AWS BAg-3. It's unique with 3% nickel. The wire is quite hard, I don't know if that's the result of work hardening from drawing.
 